Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of HERAFLEX E 6521 1000 NT - TPC - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for HERAFLEX E 6521 1000 NT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Heraflex E datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
TPC-ET Thermoplastic Elastomer. Medium-high Modulus, Nominal Shore D/15s 57. Natural colou
Механические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 390 МПа ISO 527
Напряжение в точке текучести 25 МПа ISO 527
Удлинение в точке текучести 25 % ISO 527
Номинальное удлинение при разрыве >50 % ISO 527
Ударная вязкость по Шарпи с надрезом, +23°C 70 кДж/м2 ISO 179/1eA
Напряжение при 10%-ном растяжении 19 МПа ISO 527
Напряжение при 100%-ном растяжении 22 МПа ISO 527
Напряжение при 300%-ном растяжении 23 МПа ISO 527
Стойкость к разрыву 241 кН/м ISO 34-1
Стокость к истиранию 20 мм³ ISO 4649
Твердость по Шору D 57 - ISO 7619-1
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 212 °C ISO 11357-1/-3
Температура изгиба под нагрузкой, 1.80 МПа 60 °C ISO 75-1/-2
Температура изгиба под нагрузкой, 0.45 МПа 110 °C ISO 75-1/-2
Температура размягчения по Вика, B 195 °C ISO 306
Электрические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Удельное объемное сопротивление 1E13 Ом*м IEC 62631-3-1
Прочие свойстваЗначениеЕдиницаСтандарт
Водопоглощение 0.2 % Sim. to ISO 62
Плотность 1230 кг/м³ ISO 1183
Особые свойства и характеристики
Способы переработки
Литье под давлением, Экструзия профилированных изделий
Вид поставки
Мелкие гранулы, Натуральный цвет
Доступность материала по регионам
Другая текстовая информация
Литье под давлением
The material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.05%. Typical conditions with a desiccant drier: temperature 110 ° C, dew point -30 ° C or below, time 2-4 h or more. Special care must be taken to avoid moisture absorption and contamination with other polymers when adding regrind material. Colour variation and mechanical properties reduction may occur and should always be carefully monitored.

Injection Molding Processing Parameters
Melt TemperatureMold TemperatureInjection Speed
230 - 240°C 30 - 50°Cmedium
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.